(PDF) Two-Dimensional Polyacrylamide Gel . For discontinuous systems which employ a stacking gel (e.g., Laemmli system), optimal polymerization of the overlaid lower gel (resolving gel) is achieved when visible gelation takes place 1520 min after the addition of the initiators ammonium persulfate and TEMED (note that polymerization continues long after visible gelation takes place; see Figure 1).